Abstract
To study glass/epoxy fiber orientation effects on translaminar fracture toughness under Mixed mode(I/II) load using asymmetric Four Point Bend specimen. Fracture toughness values for different fiber-oriented glass/epoxy laminates under Mixed modes are compared with unidirectional glass/epoxy laminates. Specimens were fabricated using hand layup technique with (0/45)° and (0/90)° fiber oriented glass fiber. The experimental study was conducted for 6 crack positions varying from 0 to 1 with an increment of 0.2 for Four Point Bend specimen. The specimens were tested under universal testing machine to obtain peak loads and further evaluate fracture toughness. The experimental test results show fracture toughness can be increased by orienting the fiber in the laminate. Fracture toughness is highly dominating for (0/90)° fiber-oriented laminates compared to 0° and (0/45)° glass/epoxy laminates.
Keywords
Article history
- ReceivedUntil the next stage: 22 days
- Revision requestedUntil the next stage: 11 days
- RevisedUntil the next stage: 0 days
- AcceptedUntil the next stage: 55 days
- Published
How to cite
APA
IEEE
MLA
Chicago
Harvard
Vancouver
BibTeX
RIS
Licence
May be shared and adapted, provided appropriate credit is given. Copyright © 2020 Abilash Desai, C. M. Sharanaprabhu, S. K. Kudari.
Copyright
Authors are allowed to retain both the copyright and the publishing rights of their articles without restrictions.
Open Access Statement
Fracture and Structural Integrity (F&SI) is an open-access journal which means that all content is freely available without charge to the user or his/her institution. Users are allowed to read, download, copy, distribute, print, search, or link to the full texts of the articles in this journal without asking prior permission from the publisher or the author. This is in accordance with the DOAI definition of open access.
F&SI operates under the Creative Commons Licence Attribution 4.0 International (CC-BY 4.0). This allows to copy and redistribute the material in any medium or format, to remix, transform and build upon the material for any purpose, even commercially, but giving appropriate credit, providing a link to the license, and indicating if changes were made.
Similar articles
Most read articles by the same author(s)
- S. K. Kudari, K.G. Kodancha, On the relationship between J-integral and CTOD for CT and SENB specimens , Fracture and Structural Integrity: Vol 2 No 6 (2008): October 2008
- K. G. Kodancha, S. K. Kudari, Variation of stress intensity factor and elastic T-stress along the crack-front in finite thickness plates , Fracture and Structural Integrity: Vol 3 No 8 (2009): April 2009
- S. K. Kudari, K. G. Kodancha, 3D Stress intensity factor and T-stresses (T11 and T33) formulations for a Compact Tension specimen , Fracture and Structural Integrity: Vol 11 No 39 (2017): January 2017
- M. S. Raviraj, C. M. Sharanaprabhu, G. C. Mohankumar, Experimental investigation of effect of specimen thickness on fracture toughness of Al-TiC composites , Fracture and Structural Integrity: Vol 10 No 37 (2016): July 2016
- S. K. Kudari, K. G. Kodancha, A new formulation for estimating maximum stress intensity factor at the mid plane of a SENB specimen: Study based on 3D FEA , Fracture and Structural Integrity: Vol 8 No 29 (2014): July 2014
- E. Ashoka, C. M. Sharanaprabhu, G. Kodancha Krishnaraja, Effect of cenosphere and specimen crack lengths on the fracture toughness of Al6061-SiC composites , Fracture and Structural Integrity: Vol 16 No 61 (2022): July 2022
- S. K. Kudari, B. Maiti, K. K. Ray, Experimental investigation on possible dependence of plastic zone size on specimen geometry , Fracture and Structural Integrity: Vol 3 No 7 (2009): January 2009