Abstract
The paper delivers a critical review of the research data on the crack initiation and crack growth patterns characteristic of the components of the spline-bolted joints between the propeller shaft and reducer shaft at An-24, An-26, and Il-18 aircrafts. Cracks in the shafts nucleated because of reduced bolt-fastening force. Actually, the bolt (bolts) failed first (also by fatigue) and then fatigue cracks nucleated and grew in the shafts, the spline surface fretting zones and/or sharp edges of the attachment (bolt-conducting) holes making the crack origin sites. The crack growth history shows itself through the regular Macro-Beach Marks, each mark
sequentially pointing to the next loading event of the propeller shaft, i.e., to each next flight. The cracks cease
growing for some while in the airscrews and their shafts just replaced to another aircraft. For the airscrew shafts, the critically assessed data show the crack growth period Np ranging as five to ten percent of a total
running period Nf . We recommend performing nondestructive inspection of the airscrew shafts on every 250-
hour running period to ensure the safety flights.
Keywords
Article history
- ReceivedUntil the next stage: 0 days
- AcceptedUntil the next stage: 0 days
- Published
How to cite
APA
IEEE
MLA
Chicago
Harvard
Vancouver
BibTeX
RIS
Licence
Copyright © 2014 Fracture and Structural Integrity.
Copyright
Authors are allowed to retain both the copyright and the publishing rights of their articles without restrictions.
Open Access Statement
Fracture and Structural Integrity (F&SI) is an open-access journal which means that all content is freely available without charge to the user or his/her institution. Users are allowed to read, download, copy, distribute, print, search, or link to the full texts of the articles in this journal without asking prior permission from the publisher or the author. This is in accordance with the DOAI definition of open access.
F&SI operates under the Creative Commons Licence Attribution 4.0 International (CC-BY 4.0). This allows to copy and redistribute the material in any medium or format, to remix, transform and build upon the material for any purpose, even commercially, but giving appropriate credit, providing a link to the license, and indicating if changes were made.
Similar articles
Most read articles by the same author(s)
- A. Shanyavskiy, Crack path for run-out specimens in fatigue tests: is it belonging to high- or very-high-cycle fatigue regime? , Fracture and Structural Integrity: Vol 9 No 34 (2015): October 2015
- A. Shanyavskiy, A. Toushentsov, Multiaxial fatigue of in-service aluminium longerons for helicopter rotor-blades , Fracture and Structural Integrity: Vol 10 No 37 (2016): July 2016
- A. Nikitin, C. Bathias, T. Palin-Luc, A. Shanyavskiy, Crack path in aeronautical titanium alloy under ultrasonic torsion loading , Fracture and Structural Integrity: Vol 10 No 35 (2016): January 2016
- A. Shanyavskiy, Spherical particles formation under biaxial cyclic loading due to mesotunneling effect , Fracture and Structural Integrity: Vol 9 No 33 (2015): July 2015
- A. Shanyavskiy, A. Toushentsov, Multiaxial fatigue of in-service aluminium longerons for helicopter rotor-blades , Fracture and Structural Integrity: Vol 10 No 38 (2016): October 2016